沙佰PC/ABS C2950-111

供应商
东莞市业强塑胶原料有限公司
认证
品牌
注塑合金料
型号
C2950-111
产地
沙特基础工业公司
联系电话
0769-22103662
手机号
18025120985
销售经理
刘洋平
所在地
东莞市樟木头塑金国际15栋
更新时间
2024-12-23 08:00

详细介绍

 liquid causticsoda is a kind of severe alkali inorganic chemical, which exposesas li clear solution with no color and no odor. it isintensively utilized in ordinary chemical plant with m.w. 40.1,b.p. 1388℃. it is generally called as caustic soda, viscous li well moisture absorption for water, carbon dioxide andchlorine. liquid caustic soda can not burn, but tends to corrodezinc, aluminum, copper and lead to produce hydrogen. in accordancewith re, it is processed as flaked caustic and micropearlscaustic by heat evaporation. liquid caustic soda of formosaplastics is completely manufactured from ion exchange membraneprocess to sell around all over the world and by domesticfood additives and various international surveillanceactivities.

销售热线:8

 pc/abs沙比克c2950-111(c2950-701黑色)pc/abs型号种类繁多,在此不一一列举。本公司服务宗旨:以质量求生存,以服务求信誉,以信誉迎客户,以客户求发展!欢迎各地新老客户来电来函咨询洽谈订购


pc塑料 - 物理性质

  比重:1.18-1.20克/立方厘米 成型收缩率:0.5-0.8% 成型温度:230-320℃ 干燥条件:110-120℃8小时 可在 -60~120℃下长期使用。

  物料性能冲击强度高,尺寸稳定性好,无色透明,着色性好,电绝缘性、耐腐蚀性、耐磨性好,但自润滑性差,有应力开裂倾向,高温易水解,与其它树脂相溶性差。适于制作仪表小零件、绝缘透明件和耐冲击零件

  材料特性1.无定形料,热稳定性好,成型温度范围宽,流动性差。吸湿小,但对水敏感,须经干燥处理。成型收缩率小,易发生熔融开裂和应力集中,故应严格控制成型条件,塑件须经退火处理。

  2.熔融温度高,粘度高,大于200g的塑件,宜用加热式的延伸喷嘴。

  3.塑胶流动性差,模具浇注系统以粗、短为原则,宜设冷料井,浇口宜取大,模具宜加热。

  4.料温过低会造成缺料,塑件无光泽,料温过高易溢边,塑件起泡。模温低时收缩率小、伸长率小、抗冲击强度低,抗弯、抗压、抗张强度低。模温超过120度时塑件冷却慢,易变形粘模

  5.塑件壁不宜太厚,应均匀,避免有尖角和缺口

基础创新C2950,PC/ABS沙佰基础C2950-111,PC/ABS(南沙) C2950-111